Pergunta
Pra que serve essa pedra?
http://cgi.ebay.com/Razor-Sharpening-Stone-ORIGNAL-ARCANSAS-/320566069256?pt=AU_VanityPerfumeShaving&hash=item4aa33a0808#shId

É só olhar o grit dela que tu vais saber para que serve. O desta é 6000-8000, grit alto, pedra fina, serve para afiar navalhas que já tem fio mas este está "cego"! Por que os dois valores? Por ela ser uma pedra natural e não se ter uma precisão na graduação!
Após ela, usa uma 12000 ou já vais pro strop!

Mas ela cabe na palma da mão. Olhe as dimensões:
-Dimensions: 100 x 30 mm x 10 mm
Eduardo Zaneti 
Paraná - Brasil

Offline JLTG

  • Aspirante a ajudante de auxiliar de aprendiz
  • Moderador Emérito
  • Trade Count: (+6)
  • D.Quijote de La Toja
  • **************************************************
  • Posts: 11138
    • Email
Re:Pedras para afiação
« Reply #31 on: March 26, 2011, 02:43:27 pm »
Com certeza!
Aí tu faz os movimentos em X.
José Luís Tomé Gonçalves

“Elogie em público e corrija em particular. Um líder corrige sem ofender e orienta sem humilhar." - Mario Sergio Cortella

“Se cortar, espirra sangue!” - José Luiz da Costa Gonçalves

Offline a_soares

  • Trade Count: (0)
  • Cella na tigela
  • ***********
  • Posts: 418
  • Rei do face lathering fail!
Re:Pedras para afiação
« Reply #32 on: March 26, 2011, 07:37:06 pm »
Essas Arkansas Stones são utilizadas principalmente para afiar bisturis cirúrgicos, o que explica as dimensões. Contudo também servem para afiar navalhas. Como disse o José Luís, é preciso usar o padrão em X.
Saudações, Augusto.

Offline JLTG

  • Aspirante a ajudante de auxiliar de aprendiz
  • Moderador Emérito
  • Trade Count: (+6)
  • D.Quijote de La Toja
  • **************************************************
  • Posts: 11138
    • Email
Re:Pedras para afiação
« Reply #33 on: March 26, 2011, 07:53:39 pm »
Na última vez que  estive com o callega, em Bento Bonçalves, tive a oportunidade de experimentar uma pedra destas, pequena assim e translúcida, parecendo um pedaço de vidro, o que achei que fosse a príncipio! Então, o professor me explicou o que era, de onde vinha, para que servia e pude dar uma passadinha numa navalha.
José Luís Tomé Gonçalves

“Elogie em público e corrija em particular. Um líder corrige sem ofender e orienta sem humilhar." - Mario Sergio Cortella

“Se cortar, espirra sangue!” - José Luiz da Costa Gonçalves

Offline callega

  • Trade Count: (0)
  • Maçarico
  • *
  • Posts: 0
    • meu site de cutelaria custom
Re:Pedras para afiação
« Reply #34 on: March 27, 2011, 12:50:07 am »
A minha translúcida, tenho usado após a preta.
A preta, ganhei do Olimpio. Era do pai dele. Detalhe, o Olimpio é o dono do terreno onde tá o container. Ele tem 85 anos. A preta é gande, deve ter mais de 20cm de comprimento.
A tanslúcida tem no Brasil. Santareli . Uma fornitura do interior de São Paulo.
Também tenho dois jogos combinados arkansas grandes, soft branca, hard preta (mais pra cinza, do que a outra preta antiga).
Hoje tenho usado uma xingling 13k, após uma coticule amarela pequena e uma barber hone.  Alem de strops com pasta diamantada 1micron e 0.5 micron(15k), pastas para polimento de ouro (branca) etc.
Uma coisa que tem funcionado muito bem é a xingling com slur da coticule. Depois a barber hone. Uma stropadinha no pau de pita.
Strops, tenho muitos..........
Comprei uma Naniwa 10k, que ainda nao chegou. É cerâmica.
E tambem ainda nao chegou uma coticule maior amarela e azul.
Em grâos maiores, tenho muita diamantada, até 1200. E uma cerâmica DMT 2200.
Conforme o estado, sigo a sequência diamantada ate 1200, 2200 cerâmica, arkansas preta e translúcida, xingling e barberhone.
Ou arkansas branca soft,  preta cinza, preta antiga,  translúcida, xingling e barber.
Strops no final.
« Last Edit: March 27, 2011, 02:48:19 am by jltgonca »
"... mais inteligente é aquele que sabe que não sabe..."Sócrates

http://www.callega.com
Bento Gonçalves RS
BRASIL

Offline callega

  • Trade Count: (0)
  • Maçarico
  • *
  • Posts: 0
    • meu site de cutelaria custom
Re:Pedras para afiação
« Reply #35 on: March 27, 2011, 12:56:50 am »
Esta é uma mto interessante tambem
http://cgi.ebay.com/ws/eBayISAPI.dll?ViewItem&item=380321103022&ssPageName=STRK:MEWAX:IT
Esta aqui, meu Deus..
http://cgi.ebay.com/VINTAGE-JAPANESE-AKAPIN-SUITA-TENNIN-TOISSHI-SHARPENING_W0QQitemZ260747611346QQcategoryZ35992QQcmdZViewItemQQ_trksidZp4012.m444QQ_trkparmsZalgo%3DCRX%26its%3DC%252BS%26itu%3DSI%252BUA%252BLM%252BLA%26otn%3D12%26ps%3D63%26clkid%3D8020370395091435141

O texto é muito interessante. Tenho certeza que o tipo do grao influi muito. Os sinteticos riscam mais que os naturais. Uma pedra 10k natural e uma sitetica (principalemten as diamantadas) produzem resultados completamente distintos. As ultimas riscam muuuito mais.. Vejam o final do texto.


BONUS SLURRY STONES INCLUDED! (1 EACH TAKASHIMA & UCHIGUMORI NAGURA)

You are looking at a Akapin Suita, pre WW2 Japanese sharpening stone. Before WW2 stones were hand cut and after WW2 they used large circlular saws. This is the highest quality Akapin, red, stone. Find out for yourself the legend of the akapin..  Size 194X71X29mm weighing 920grams. It is from  the mountains of Kyoto, Japan. it will leave a beautiful mist and haze finish. This stone is a softer very fine grain and very abrasive grit with a good positive feedback that will polishe to a beautiful mist and haze.Japanese tennin toishi were graded thoughout history for samurai swords, they work equally well for the finest of razors. Here is a perfect finish stone and being softer is a very good beginers stone yet with more than enough fine grain and brute abrasive power for a master.  With a little practice you will be amazed at how sharp you can hone your fine blade. You can use it with or without slurry and it will give fantastic results.  Notice the iron flower in the picture showing the iron particles in the slurry.

HGAL 3++3++++3+++3++++

H is the hardness of the stone is based on a scale of 5

G is the grain, how fine the grain on a scale of 3

A is the abrasive power of the stone on a scale of 3

L is the lightness, the feel of the stones feedback on a scale of 3

 

I have been asked what grit these stones are and that is a very hard question to answer. The beauty of the Tennen Toishi is that it may cut like an 8000 grit stone but the longer you use it and the slurry builds, the grit size breaks down and some stones will polish with smaller particles than a 30,000 grit Shapton. With a very high grade stone like this one, you end up with a beautiful mist and haze that no artificial stone can match.
« Last Edit: March 27, 2011, 02:08:58 am by callega »
"... mais inteligente é aquele que sabe que não sabe..."Sócrates

http://www.callega.com
Bento Gonçalves RS
BRASIL

Offline JLTG

  • Aspirante a ajudante de auxiliar de aprendiz
  • Moderador Emérito
  • Trade Count: (+6)
  • D.Quijote de La Toja
  • **************************************************
  • Posts: 11138
    • Email
Re:Pedras para afiação
« Reply #36 on: March 27, 2011, 02:39:05 am »
Essa última podíamos mandar vir umas 10?
José Luís Tomé Gonçalves

“Elogie em público e corrija em particular. Um líder corrige sem ofender e orienta sem humilhar." - Mario Sergio Cortella

“Se cortar, espirra sangue!” - José Luiz da Costa Gonçalves

Offline callega

  • Trade Count: (0)
  • Maçarico
  • *
  • Posts: 0
    • meu site de cutelaria custom
Re:Pedras para afiação
« Reply #37 on: March 27, 2011, 10:56:06 am »
Duzias??
10 duzias??
"... mais inteligente é aquele que sabe que não sabe..."Sócrates

http://www.callega.com
Bento Gonçalves RS
BRASIL

Offline callega

  • Trade Count: (0)
  • Maçarico
  • *
  • Posts: 0
    • meu site de cutelaria custom
Re:Pedras para afiação
« Reply #38 on: September 20, 2011, 12:26:23 am »
Revivendo e vendo como a zente "evolói">
É aqui que o Cegadede diz que a arkansas nao funcia pra navalha.
Mas eu acho qeu indo alem dela, é melhor.
"... mais inteligente é aquele que sabe que não sabe..."Sócrates

http://www.callega.com
Bento Gonçalves RS
BRASIL

Offline GADREL

  • Trade Count: (0)
  • D.Quijote de La Toja
  • ********************************************
  • Posts: 10037
  • São Paulo, Brasil.
    • Email
Re:Pedras para afiação
« Reply #39 on: September 20, 2011, 08:56:38 am »
LEGIO PATRIA NOSTRA.

Offline nunovix

  • Trade Count: (0)
  • Faz 444 passagens
  • ********
  • Posts: 210
    • Email
Re:Pedras para afiação
« Reply #40 on: February 10, 2012, 10:01:35 pm »
Alguém sabe qual é a dureza destas "pedras" de diamante e cerâmica?

Fallkniven DC4 Combination Sharpening Stone
http://www.thebushcraftstore.co.uk/fallkniven-dc4-combination-sharpening-stone-3986-p.asp

Offline GADREL

  • Trade Count: (0)
  • D.Quijote de La Toja
  • ********************************************
  • Posts: 10037
  • São Paulo, Brasil.
    • Email
Re:Pedras para afiação
« Reply #41 on: February 10, 2012, 10:08:39 pm »
Alguém sabe qual é a dureza destas "pedras" de diamante e cerâmica?

Fallkniven DC4 Combination Sharpening Stone
http://www.thebushcraftstore.co.uk/fallkniven-dc4-combination-sharpening-stone-3986-p.asp
A dureza é a mesma dos materiais que a compõe.
LEGIO PATRIA NOSTRA.

Offline nunovix

  • Trade Count: (0)
  • Faz 444 passagens
  • ********
  • Posts: 210
    • Email
Re:Pedras para afiação
« Reply #42 on: February 10, 2012, 10:18:01 pm »

Mas em graus...é equivalente a uma Japanese waterstone 1000, 2000, 3000?

Offline callega

  • Trade Count: (0)
  • Maçarico
  • *
  • Posts: 0
    • meu site de cutelaria custom
Re:Pedras para afiação
« Reply #43 on: February 10, 2012, 10:27:21 pm »
Amigo, falas das ceramicas japonesas? sao moles . Diamante é o material mais duro que se conhece.
Em pedras de afiação, so escutei falar em dureza da pedra qdo se fala em pedras naturais japonesas. Qdomais profundas, mais duras. Sim, um pouco se fala nas coticule tambem.. Mas para por ai.
"... mais inteligente é aquele que sabe que não sabe..."Sócrates

http://www.callega.com
Bento Gonçalves RS
BRASIL

Offline GADREL

  • Trade Count: (0)
  • D.Quijote de La Toja
  • ********************************************
  • Posts: 10037
  • São Paulo, Brasil.
    • Email
Re:Pedras para afiação
« Reply #44 on: February 10, 2012, 10:37:04 pm »

Mas em graus...é equivalente a uma Japanese waterstone 1000, 2000, 3000?

Fazes, então, referência ao grit, que se refere ao tamanho de grão das partículas na pedra.